Seven skills of reducing defects in mold processing

Release time:2025-06-11

In order to improve the performance of molds, many manufacturers will properly process their own molds. Mold processing refers to the processing of forming and blank making tools, including shear molds and die-cutting molds. However, in many cases, processing defects will be reflected after mold processing, resulting in the decline of mold performance. How to construct mold processing defects, the following seven measures can be taken to build mold processing defects.


1. For the reasonable selection and dressing of grinding wheel, white corundum grinding wheel is better, its performance is hard and brittle, and it is easy to produce new cutting edges. Therefore, the cutting force is small, the grinding heat is small, and the use of medium grain size, such as 46~60 mesh, is better. The hardness of the grinding wheel adopts medium soft and soft (ZR1, Zr2 and R1, R2), that is, the low hardness, coarse grain grinding wheel, which has good self excitation and can reduce the cutting heat.

It is very important to choose a suitable grinding wheel for fine grinding. In view of the high vanadium and molybdenum content of die steel, Gd single crystal corundum grinding wheel is more suitable. When machining cemented carbide and materials with high quenching hardness, organic bonded diamond grinding wheel is preferred. Organic bonded grinding wheel has good self grinding performance, and the workpiece roughness can reach Ra0.2 μ m. In recent years, with the application of new materials, CBN (cubic boron nitride) grinding wheel has shown good processing effect. When it is processed on CNC forming grinder, coordinate grinder, CNC CNC Internal and external grinder, its processing effect is better than other kinds of grinding wheels.

During grinding, the grinding wheel should be trimmed in time to keep it sharp. When the grinding wheel is passivated, it will rub and squeeze on the surface of the workpiece, resulting in surface burns and strength reduction.


2. Use cooling lubricant reasonably, give play to the three functions of cooling, washing and lubrication, keep the cooling and lubrication clean, control the grinding heat within the allowable range, and prevent the thermal deformation of the workpiece. Improve the cooling conditions during grinding, such as using oil impregnated grinding wheel or internally cooled grinding wheel. When the cutting fluid is introduced into the center of the grinding wheel, the cutting fluid can directly enter the grinding area, which plays an effective cooling role and prevents the workpiece surface from being burned.


3. After heat treatment, the quenching stress shall be minimized, because the quenching stress and network carbonization structure are under the action of grinding force, and the workpiece is easy to crack due to the phase transformation of the structure. For high-precision dies, in order to remove the residual stress of grinding, low-temperature aging treatment should be carried out after grinding to improve the toughness.


4. In order to remove the grinding stress, the mold can also be soaked in a salt bath at 260 ℃ ~315 ℃ for 1.5min, and then cooled in oil at 30 ℃, so that the hardness is reduced by 1hrc and the residual stress is reduced by 40%~65%.


5. For the precision grinding of precision dies with dimensional tolerance within 0.01mm, attention should be paid to the influence of ambient temperature, and constant temperature grinding is required. According to the calculation, when the temperature difference of 300mm long steel parts is 3 ℃, the material change is about 10.8 μ m (10.8=1.2 × three × 3. The deformation per 100mm is 1.2 μ M/ ℃), all finishing processes should fully consider the influence of this factor.


6. Electrolytic grinding is adopted to improve the precision and surface quality of mold manufacturing. During electrolytic grinding, the grinding wheel scrapes off the oxide film instead of grinding the metal, so the grinding force is small, the grinding heat is small, and there will be no grinding burrs, cracks, burns and other phenomena. Generally, the surface roughness can be better than ra0.16 microns; In addition, the wear of grinding wheel is set to be small. For example, when grinding cemented carbide, the wear of silicon carbide grinding wheel is about 400% - 600% of the weight of cemented carbide, while in electrolytic grinding, the wear of grinding wheel is only 50% - 100% of cemented carbide.


7. Select the grinding amount reasonably, and adopt the fine grinding method of small radial feed and even fine grinding. If the radial feed rate and the speed of the grinding wheel are properly reduced, and the axial feed rate is increased, the contact area between the grinding wheel and the workpiece will be reduced, and the heat dissipation conditions will be improved, so as to effectively control the increase of the surface temperature.


Copyright: Shenzhen Zhongyuan Plastic Co., Ltd. | mold processing customized manufacturer. If you want to know the processing price of the factory, how much is it, and which is good, please contact us Yue ICP Bei No. 17060480
白嫩无码人妻丰满熟妇啪啪区百度| 欧美交a欧美精品喷水| 人与动性xxxxx免费| 爱豆传媒在线视频观看网站入口| 免费污视频在线| 波多野结衣护士无删减| 亚洲视频在线观看不卡| 欧美日韩国产区在线观看| 亚洲日韩久久综合中文字幕| 欧洲精品无码一区二区三区在线播放 | 苍井空亚洲精品AA片在线播放| 国产免费久久精品久久久| 色噜噜狠狠一区二区三区| 国产一区在线mmai| 精品一区二区三区影院在线午夜| 免费看国产一级特黄aa大片| 欧美色欧美亚洲高清在线观看| 亚洲熟妇色xxxxx欧美老妇| 最近高清中文在线国语字幕| 亚洲av丰满熟妇在线播放| 日本三级香港三级人妇99视| 久久久久亚洲AV成人网人人网站| 少妇高潮无套内谢| www视频在线观看天堂| 国产精品资源在线| 1024国产视频| 国产午夜精品一二区理论影院| 精品国产福利片在线观看 | 午夜精品久久久久久久99热| 深爱婷婷激情网| 亚洲欧美日韩中文无线码| 日韩精品无码一本二本三本 | 久久精品一本到99热免费| 成都4片p高清视频| 一区二区三区四区视频| 国产精品美女久久久网av| 韩国成人在线视频| 四虎精品成人免费影视| 激情网站免费看| 亚洲国产欧洲综合997久久| 日本理论在线看片|